GLOSSINESS COLOR STABILITY AND SURFACE ROUGHNESS OF WOOD TREATED WITHSOME BLEACHING CHEMICALS
Yazarlar (7)
Prof. Dr. Ayhan Özçifçi Aksaray Üniversitesi, Türkiye
Fatih Yapıcı Ondokuz Mayıs Üniversitesi, Türkiye
Prof. Dr. Suat ALTUN Karabük Üniversitesi, Türkiye
Prof. Dr. Hilmi Toker Muğla Sıtkı Koçman Üniversitesi, Türkiye
Prof. Dr. Ergün Baysal Muğla Sıtkı Koçman Üniversitesi, Türkiye
Ahmet Şenel
Gazi Üniversitesi, Türkiye
Hakan Şimşek Gaziosmanpaşa Üniversitesi, Türkiye
Makale Türü Özgün Makale (SSCI, AHCI, SCI, SCI-Exp dergilerinde yayınlanan tam makale)
Dergi Adı Wood Research (Q3)
Dergi ISSN 1336-4561 Dergi Bilgileri (2009)
Dergi Tarandığı Indeksler SCI-Expanded
Makale Dili İngilizce Basım Tarihi 04-2009
Cilt / Sayı / Sayfa 54 / 2 / 83–94 DOI
UAK Araştırma Alanları
Ahşap Esaslı Kompozitler
Özet
The aim of this study was to determine the effects of different bleaching chemicals and their treatment time on glossiness, color stability, and surface roughness of wood. Spruce (Picea orientalis L.) and oak (Quercus sessiliflora Salisb.) wood specimens were bleached with aqueous solutions of 25% hydrogen peroxide (H2O2), 25% ammonia (NH3), and their mixture (1: 1; volume: volume) for 10, 20, and 30 minutes immersing. Glossiness of wood specimens parallel and perpendicular to grain values were measured with Glossmeter at 60-degree incident angle. Color measurements and surface roughness were wade according to ISO 7724–2, and ISO 4287 standards, respectively. Results showed that the highest glossiness decrease (0.99) was observed in oak wood treated with ammonia solution perpendicular to grain for 20 min. immersing. The highest total color chance (18.88) was observed in oak wood treated with ammonia solution for 30 minutes immersing. All bleaching solutions increased the surface roughness of wood specimens.
Anahtar Kelimeler
Bleaching | Glossiness color stability | Surface roughness | Wood